Electrolyte for cell using LiMn2O4 as cathode material JM-01
Application
- This product is designed for cell using LiMn2O4 as cathode material and artificial or natural graphite as anode material.
- The cell using it will have good cycle life and good performance at high temperature.
Composition
| Ester solvents | LiPF6 | additive, etc. |
Specification
| Item | Spec. | Testing Method |
|---|---|---|
| Colority | ≤ 20 Hazen | Pt/Co scale |
| Water | ≤ 20 ppm | Karl-Fischer titration |
| Free acid (as HF) | ≤ 50 ppm | Neutralization |
| Metal | ≤ 10 ppm | Atomic Absorption |
| Density(25℃) | 1.21±0.03 g/cm3 | Pycnometer |
| Conductivity(25℃) | 7.5±0.5 mS/cm | Conductivity meter |
Custom Test Result
| Charge-discharge efficiency at first cycle (%) | Capacity retention at ambient temperature (%) | Discharges platform maintenance rate (%) | Expansion rate | |||
|---|---|---|---|---|---|---|
| 100 cycle | 200 cycle | 100 cycle | 200 cycle | 100 cycle | 200 cycle | |
| >90 | >98 | >95 | >98.5 | >96.5 | <1 | <3 |
Electrolyte for cell using LiMn2O4 as cathode material JM-03
Application
- This product is designed for cell using LiMn2O4 as cathode material and artificial graphite as anode material.
- The cell using it will have good cycle life and good performance at high temperature.
Composition
| Ester solvents | LiPF6 | additive, etc. |
Specification
| Item | Spec. | Testing Method |
|---|---|---|
| Colority | ≤ 20 Hazen | Pt/Co scale |
| Water | ≤ 20 ppm | Karl-Fischer titration |
| Free acid (as HF) | ≤ 50 ppm | Neutralization |
| Metal | ≤ 10 ppm | Atomic Absorption |
| Density(25℃) | 1.24±0.03 g/cm3 | Pycnometer |
| Conductivity(25℃) | 10.5±0.5 mS/cm | Conductivity meter |
Custom Test Result
| Charge-discharge efficiency at first cycle (%) | Capacity retention at ambient temperature (%) | Discharges platform maintenance rate (%) | Expansion rate | |||
|---|---|---|---|---|---|---|
| 100 cycle | 200 cycle | 100 cycle | 200 cycle | 100 cycle | 200 cycle | |
| >92 | >95 | >93 | >99 | >97.5 | <1 | <5 |
Electrolyte for cell using LiMn2O4 as cathode material JM-04
Application
- This product is designed for cell using LiMn2O4 as cathode material and artificial graphite as anode material.
- The cell using it will have good cycle life and good performance at high temperature.
Composition
| Ester solvents | LiPF6 | additive, etc. |
Specification
| Item | Spec. | Testing Method |
|---|---|---|
| Colority | ≤ 20 Hazen | Pt/Co scale |
| Water | ≤ 20 ppm | Karl-Fischer titration |
| Free acid (as HF) | ≤ 50 ppm | Neutralization |
| Metal | ≤ 10 ppm | Atomic Absorption |
| Density(25℃) | 1.21±0.03 g/cm3 | Pycnometer |
| Conductivity(25℃) | 10.5±0.5 mS/cm | Conductivity meter |
Custom Test Result
| Charge-discharge efficiency at first cycle (%) | Capacity retention at ambient temperature (%) | Discharges platform maintenance rate (%) | Expansion rate | |||
|---|---|---|---|---|---|---|
| 100 cycle | 200 cycle | 100 cycle | 200 cycle | 100 cycle | 200 cycle | |
| >90 | >96 | >94 | >99.5 | >97.5 | <1 | <3 |